Indium tin oxide (I.T.O)
|
Formula
|
In2O3 + SnO2
|
|
Evaporation temperature
|
1400-1500°C
|
|
Transmission range
|
400-1000nm
|
|
Refractive index
|
2.0 at 500nm
|
|
Evaporation source
|
E, Al2O3
|
|
Notes on application
|
Conductive transparent layers
|
Order information
|
Cat. Number
|
Specification
|
Standard packages
|
|
Cat No. 7011
|
Tablets Ø 6.5 x 7t
|
100g
|
|
Cat No. 7012
|
Tablets Ø 10.25 x 8.4t
|
100g
|
|
|
|
Material |
ITO powder |
Packaging |
100g/1pack |
Delivery lead time |
1week |
Minimum order |
100g/1pack |
Supply ability |